TM  55-1520-240-23-8 10-15.1 REPAIR  FUEL  CELL  INTERIOR PLIES (Continued) 10-15.1 Keep  lid  on  can  of  barrier  cement (E63.3)  when  not  in  use  to  prevent evaporation  and  thickening. i. Carefully  apply  a  uniform  coat  of  barrier cement  (E63.3)  (5)  over  previous  coat  of repair  cement mixture  (6).   Use  a  brush  (7). Remove  any  excess cement  from  unbuffed area.   Use  a  clean  cloth  (E120)  and  MEK (E244).  Wear  gloves  (E184.1).  Allow  barrier to  dry  to  touch. j. Apply  a  second  coat  of barrier  cement  (8) over  first coat at 90º  to  the  application  of  the first coat.  Use  a  brush.  Allow  second  coat  to air  dry  for  30  minutes. k. Prepare  repair  cement  (E63.3).  (See  steps e  and  f.) l. Carefully  apply  a  uniform  coat  to  repair cement  (9)  over  previous  coats  of  barrier cement.   Smooth  surface  with  MEK  (E244) and  remove  any  excess  cement  from unbuffed  area  with  a  clean  cloth  (E120)  and MEK (E244).  Wear  gloves  (E184.1). m. Wet  fabric reinforcement patch  (2)  with  MEK (E244).  Shake  out excess MEK  (E244). n. Center  wet  patch  over  defect area  and  press into  wet  cement  (9)  with  fingers  to  make certain  patch  is  free  of  air  bubbles and  loose edges. o. Allow  cement  and  fabric  patch  to  air  cure approximately 30 minutes. 10-63