TM  55-1520-240-23-8 10-10 FUEL  CELL DAMAGE  —  CLASSIFICATION  AND  REPAIR  LIMITS  (GENERAL INFORMATION) 10-10 INITIAL  SETUP Applicable Configurations: All Tools: None Materials: Repair Cement  —  2  Part  Set  (E63.2) Personnel  Required: Inspector References: Task  10-7 Task  10-8 Task  10-11 Task  10-12 Task  10-15 Task  10-15.1 Task  10-24 Task  10-29 Equipment  Condition: Off  Helicopter Remove  fuel cell  from  helicopter  and clean  before  doing  any repair  (Task 10-7, 10-24  or 10-29  and  10-8). 1. Classify  fuel cell  damage  as follows: MINOR DAMAGE 2. No  repair is required  if  damage  is  confined  to: a. Blisters less  than  1 inch  diameter. b. Loose  lap  seam  with  1  inch  (minimum) effective  seal  after removal  of  loose  edges. REPARABLE  DAMAGE 3. Damage  that is  reparable  is  classified  as follows: a. Blister  Damage.   Blisters exceeding  1 inch diameter  must  be  repaired.   Cut  away  the blister and  apply an  internal  or an  external cement  repair,  depending  upon  the  blister location  (Tasks  10-11  and  10-15). b. Loose  Seam  Damage.  A loose  seam  having less  than  1 inch  of  effective  seal  must  be repaired.   Remove  the  loose  edges  and apply  an  internal  or  an  external  reinforced cover  patch  depending  upon  the  loose  seam location  (Tasks  10-12  and  10-15.1). c. Cuts,  Tears,  Chafing  or  Snag  Damage.   All cuts, tears, chafing  and  snags  occuring  to  but not penetrating  inner  liner or outer  coating must  be  repaired.  Trim  the  damaged  area and  apply  an  internal or an  external  cement repair,  depending  upon  the  damage  location (Tasks 10-11  and  10-15). d. Cuts,  Tears,  Snags,  and  Holes.   All  cuts, tears,  snags  and  holes  (not  including holes  which  penetrate  the  entire  cell  wall) penetrating  one  or more  plies  require  an internal  and  external  reinforced  cover  patch, depending  on  location.   Repair  is  limited  to damages not  exceeding  a  length  or diameter of  4  inches  after  trimming.   Remove  loose material  and  ragged  edges.   Apply  external patch  first  (Tasks  10-12  and  10-15.1). e. Hole  Damage.   Holes  which  penetrate  the entire  cell  wall  without  sealant  activation and  do  not  exceed  a  length  of  4  inches. Apply external  patch  first  (Tasks  10-12  and 10-15.1). f. Loose  Fitting  Flange  Damage  (Internal  and External).  Clean  and  buff  contact  surfaces. Cement surfaces with  repair  cement (E63.2) (Tasks 10-11  and  10-15). g. Replacement  of  fitting  thread  inserts (helicoils) (TM  1-1500-204-23). 10-49