Click here to make tpub.com your Home Page

Page Title: Dissimilar Metals.
Back | Up | Next

Click here for thousands of PDF manuals

Google


Web
www.tpub.com

Home


   
Information Categories
.... Administration
Advancement
Aerographer
Automotive
Aviation
Construction
Diving
Draftsman
Engineering
Electronics
Food and Cooking
Logistics
Math
Medical
Music
Nuclear Fundamentals
Photography
Religion
   
   

 

Back
Protective Coatings
Up
TB-9-1377-200 Propellant Actuated Devices Manual
Next
Chapter 5. BALLISTIC DESIGN AND ANALYSIS

eliminated by the use of microcrystalline waxes on the
subject to galvanic corrosion, when an aluminum
surface passes over another aluminum surface, there is
sliding surfaces and teflon-coated aluminum pistons and
tubes. Teflon coatings and wax finishes also serve to
it tendency for the surfaces to gill. Galling also occurs
when a cadmium surface rubs against another cadmium
reduce friction between sliding members of propellant
actuated devices.
surface, as a cadmium plated piston sliding (stroking)
through  a  cadmium-plated  bushing.
Galling  is